Former specification for heat-treated high-strength bolts for steel structure connections. It was withdrawn in 2016 and continued as Grade A325 of ASTM F3125, but it still often remains on drawings and BOMs.

Status: Withdrawn (→ ASTM F3125 Grade A325, 2016)

Key points

  • The former standard's minimum tensile strength was 120 ksi (about 827 MPa) or 105 ksi (about 724 MPa) depending on diameter; F3125 Grade A325 is the 120 ksi class.
  • Type 1 (medium carbon steel, carbon boron steel, and alloy steel family) and Type 3 (weathering steel). It is a heavy hex structural bolt in sizes 1/2" to 1-1/2".
  • Mating parts are A563 nuts (DH, etc.) and F436 hardened washers.
  • The metric A325M and the twist-off type F1852 were also consolidated into F3125 along with it.

Checks for BOMs and buying

  • Even if you order "A325", it is normal for the certificate to read "F3125 Grade A325". It is not nonconforming because the standard number differs.
  • Do not substitute ordinary hex bolts (including SAE grade bolts) for A325. The heavy hex head, short threaded portion, and set rotational capacity test differ.

Equivalent and superseding standards

  • ASTM F3125 Grade A325 Successor standard (consolidated into a grade)