Non-electrolytic coating in which zinc and aluminum flakes are applied with a binder and cured by heating. No hydrogen is generated during deposition, so it is used for 10.9 and 12.9 high-strength fasteners.
Status: Current
Key points
- It includes systems with and without hexavalent chromium, and with and without topcoat and lubricant. It applies to bolts, nuts, washers, pins, etc.
- No hydrogen is generated in the deposition process, and with alkaline or solvent cleaning + mechanical cleaning as pretreatment there is no risk of internal hydrogen embrittlement.
- Above 390 HV or for 12.9 and above, acid pickling must not be done. Cathodic cleaning is not permitted.
- The curing temperature rises up to 320 °C depending on the system and must not exceed the tempering temperature of quenched and tempered fasteners.
- Corrosion resistance is specified by the neutral salt spray test (ISO 9227) hours, with no red rust. Thickness is a reference value.
- The zinc flake coating standard for inch fasteners is ASTM F3393. The zinc/aluminum coating standard ASTM F1136 was withdrawn in 2025 and replaced by F3393.
Checks for BOMs and buying
- Coating thickness affects thread engagement. For thick specifications, check gauges and assembly.
- The friction coefficient changes depending on the coating type (with or without lubricating topcoat), so set the torque value again (ISO 16047 test).
- A distributor that buys uncoated fasteners and has them coated before passing them on is treated as an "alteration distributor" (ISO 1891-4 term).
- For systems containing hexavalent chromium, check whether they are subject to regulations such as RoHS.
ASTM: official search ↗ · ISO: official search ↗
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: ISO 10683 · ASTM F3393/F3393M · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.