boltnoteSend an RFQ →

Home › Standards glossary › Surface treatment and corrosion › Hydrogen embrittlement

Hydrogen embrittlement

CommonConcept

Hydrogen embrittlement (delayed fracture)

← Back to topicSend a BOM or RFQ →

A phenomenon in which a high-strength bolt, because of hydrogen that has entered the steel, suddenly fractures under a low load some time after being tightened. The higher the hardness, the greater the risk, so it is managed through the choice of plating or coating and the baking conditions.

Key points

  • It occurs when three conditions overlap: high hardness (strength), tensile stress (including clamp load), and absorbed hydrogen.
  • Internal hydrogen embrittlement (IHE) is caused by hydrogen from manufacturing processes such as pickling, electroplating and phosphating, and environmental hydrogen embrittlement (EHE) by hydrogen generated in service by corrosion, cathodic protection or H2S.
  • ISO 4042 manages it by ISO 898-1 property class. No separate measure is needed for 9.8 or below; 10.9 requires process validation and product testing, or baking; and 12.9 requires both process validation and product testing, and baking.
  • RCSC (2025) considers that bolts above a tensile strength of 180 ksi (about 39 HRC) can become embrittled if hydrogen is present and they are under high tensile stress.
  • For hot-dip galvanizing, the problem is hydrogen from pickling. ISO 10684 requires parts of 320 HV or more to be cleaned by acid with inhibitor, alkaline or mechanical methods, and covers bolts only up to 10.9.
  • Zinc flake generates no hydrogen during application, so it is mainly used on high-strength bolts of 1000 MPa or more (ISO 10683).
  • Suspect lots are checked by a test in which the parts are held in the tightened state for a set time (such as ISO 15330).

Hydrogen risk and control by surface treatment

TreatmentStage where hydrogen entersControl for high-strength parts
Electro-zinc, zinc-nickel, cadmiumPickling, platingProcess validation and baking per ISO 4042 and F1941
Phosphate coatingDuring treatmentHydrogen removal treatment if needed
Hot-dip galvanizingMainly picklingFor 320 HV or more, inhibitor acid, alkaline or mechanical cleaning; bolts up to 10.9 (ISO 10684)
Zinc flakeNone during applicationMechanical cleaning; no pickling above 12.9 or 390 HV
Black oxideDuring pretreatment and treatment (caustic embrittlement is a concern above 1000 MPa)Heat treatment before and after treatment if needed (ISO 11408)

Checks for BOMs and buying

  • For electroplating of 10.9, 12.9, SAE Grade 8 and A574, state in the purchase order whether baking is done, its conditions, and the submission of records.
  • For grades whose standard limits the coating, such as F3125 A490, use only the permitted coatings (such as zinc flake).
  • High-strength bolts in a seawater cathodic protection zone can also fracture from hydrogen generated in service, so check the hardness upper limit in the specification.
  • Delayed fracture appears after time has passed, not immediately after tightening. Do not be reassured because nothing is wrong right after assembly.

ASTM: official search ↗ · ISO: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: ISO 4042 · ASTM F1941/F1941M · ISO 10684 · ISO 10683 · ISO 15330 · ISO 11408 · RCSC Specification (2025) · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.