boltnoteSend an RFQ →

Home › Standards glossary › Surface treatment and corrosion › Zinc-nickel plating

Zinc-nickel plating

CommonCoating

Zinc-nickel alloy electroplating

← Back to topicSend a BOM or RFQ →

An electroplating of a zinc alloy mixed with nickel, with better corrosion resistance than zinc of the same thickness, used in place of plain zinc and cadmium for automotive, aerospace and plant bolting.

Key points

  • For fasteners, it is one of the plating families covered by ISO 4042, and ASTM B841 is a zinc-nickel plating standard for general parts.
  • For alkaline zinc-nickel plating with 12 to 16 % nickel, ISO 4042 allows baking of high-strength parts to be omitted if the basis is confirmed by testing and the supplier and buyer agree.
  • It is used with a hexavalent-chromium-free passivation (or chromate) and a sealer, and finishes such as clear (silver) and black are available.
  • ISO 4042 notes that acid zinc-nickel has also been reported to have benefits similar to alkaline, but considers that more data is needed to decide on omitting baking.
  • As with electro-zinc, the thickness takes up thread tolerance, so thickness is set within the 6g allowance.

Checks for BOMs and buying

  • Zinc-nickel is also electroplating. Omitting baking for 12.9 and high-hardness parts is accepted only when there is a test basis and agreement.
  • Writing only "zinc-nickel" does not set the nickel content, passivation, sealer or salt spray hours. State them together in the specification string.
  • When using it on high-temperature bolting, check the service temperature limit in the coating specification.

ASTM: official search ↗ · ISO: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: ISO 4042 · ASTM B841 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.