Electro-zinc plating (white, yellow, black)

CommonCoating

Zinc electroplating with passivation (clear, yellow, black)

← Back to topicSend a BOM or RFQ →

The most common bolt plating, in which a thin zinc layer is applied electrolytically and a conversion treatment adds color and corrosion resistance. For high-strength parts, look at hydrogen embrittlement, and for thickness, the thread tolerance.

Key points

  • The references for fastener electroplating are ISO 4042 (zinc, zinc-nickel, zinc-iron, cadmium), ASTM F1941/F1941M for inch and metric fasteners, and ASTM B633 and ISO 2081 for general steel parts.
  • Color is determined by the conversion treatment (passivation), and there are white (blue-white), yellow, black and others. Hexavalent-chromium-free treatments (trivalent chromium, etc.) are now widely used in place of hexavalent chromium.
  • ASTM B633 divides thickness into four standard grades, and the current edition (2023) also provides hexavalent-chromium-free post-treatment types.
  • On a 60° thread, the effective diameter grows by about 4 times the plating thickness. An external thread with tolerance allowance such as 6g is plated within that allowance, while a 6h thread with no allowance has its pre-plating dimension reduced or another treatment is chosen.
  • ISO 4042: no additional hydrogen-related measure is needed for 9.8 or below; 10.9 requires process validation and product testing, or baking; and 12.9 requires both.
  • The friction coefficient differs with the conversion treatment, sealer and topcoat, so the clamp load changes even at the same torque.

Colors and conversion treatments

ColorTreatmentRemarks
White (blue-white)Trivalent clear passivationNo hexavalent chromium
Yellow (iridescent)Formerly hexavalent chromate; now also trivalent treatments (including colored)For RoHS-regulated products, state "trivalent"
BlackTrivalent black passivationFor 10.9 and above, check the baking conditions

Checks for BOMs and buying

  • "YELLOW ZINC" and "colored chromate" on a drawing are notations that commonly meant a hexavalent chromium process, so for RoHS-regulated products, respecify with a hexavalent-chromium-free treatment.
  • Hexavalent and trivalent cannot be told apart by color alone. If needed, get a hexavalent chromium non-detection test result.
  • For high-hardness parts such as 10.9, 12.9, SAE Grade 8, A574 and spring washers, check the baking conditions or consider zinc flake.
  • If thick plating is required, the thread gauge may not go on even a 6g bolt. Specify thickness and thread tolerance together.

ASTM: official search ↗ · ISO: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: ISO 4042 · ASTM F1941/F1941M · ASTM B633 · ISO 2081 · ISO 10684 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.