Specification for electroplating of inch and metric threaded fasteners. It sets plating thickness, hexavalent (Cr6+) chromate and trivalent (Cr3+) chromite post-treatment, corrosion resistance, and the control and removal (baking) of hydrogen embrittlement in high-strength parts.
Status: Current
Key points
- Scope: Unified inch and metric threaded fasteners. It can also be applied to unthreaded parts such as washers and pins.
- Covers: plating thickness, hexavalent (Cr6+) chromate or non-Cr6+ (trivalent, Cr3+) conversion treatment, corrosion resistance, control of the hydrogen embrittlement risk of high-strength parts, and the removal treatment (baking).
- The current edition is a combined inch-metric edition (F1941/F1941M).
- ASTM F1940 is the test method for verifying process control of hydrogen embrittlement.
Checks for BOMs and buying
- If electroplating is specified for high-strength bolts, state the hydrogen embrittlement countermeasures (whether to bake and under what conditions) and the verification method (F1940) in the order. F1941-15 does not make baking mandatory if the specified maximum hardness is 39 HRC or less.
- If RoHS compliance is required, specify trivalent (Cr3+) treatment rather than hexavalent (Cr6+) chromate.
Equivalent and superseding standards
- ISO 4042 Metric fastener electroplating
- ASTM B633 General standard for electrogalvanizing on steel
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: ASTM F1941/F1941M · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.