A treatment in which parts are heated at a specified temperature for a specified time immediately after plating, to drive out the hydrogen that entered the steel during the plating process. It reduces the risk of hydrogen embrittlement in high-strength plated parts.
Key points
- Temperature and time are set by the process standard (ISO 9588, ASTM B850, etc.) and the order specification, according to part hardness, size and plating type.
- ISO 4042 requires baking for 12.9 (specified maximum hardness above 390 HV), and allows 10.9 to be handled by process validation and product testing instead.
- If baking is done on hot-dip galvanized parts, it is done before fluxing (surface activation) (ISO 10684).
- Whether baking was done can be confirmed only if the plating certificate records the temperature, time and start time.
Checks for BOMs and buying
- For a quotation that says only "baking included", also check the temperature, time, the deadline for starting after plating, and whether records are submitted.
- For 12.9 class, first consider another treatment that generates no hydrogen during application, such as zinc flake (ISO 10683).
- If plating is stripped and redone, the parts go through pickling and plating again, so baking is also redone.
ASTM: official search ↗ · ISO: official search ↗
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: ISO 4042 · ISO 9588 · ASTM B850 · ISO 10684 · ISO 10683 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.