The on-site term for a certificate issued by a steelmaker, material manufacturer, or bolt manufacturer stating the chemical composition and mechanical test values by heat. The document type (EN 10204 2.2, 3.1, etc.) is decided by the order, so first check who tested what, in what condition.
Key points
- A mill certificate has two layers: the material certificate of the steelmaker or bar manufacturer (heat composition, bar mechanical values) and the product certificate of the bolt or stud manufacturer (heat treatment lot, hardness, tensile, proof load, etc.).
- Composition is a value per heat (melt), and mechanical values differ by heat treatment lot and diameter. Check that the diameter and lot on the certificate match the delivered product.
- Order of reading: issuer · standard · grade · heat number → whether the composition is within the grade range → tensile · yield · elongation · reduction of area → hardness → impact (low-temperature grades) → heat treatment conditions → confirmation by the inspection representative.
Fields to check on a mill certificate
| Item | What to check |
|---|---|
| Issuer | Name and address of the original manufacturer, name, title, and confirmation of the inspection representative (independent of the manufacturing department for 3.1) |
| Standard and grade | Whether the standard number, year, and grade symbol, such as ASTM A193/A193M B7, are the same as the order |
| Heat number | Whether it is the same as the number on the product marking, label, and packaging |
| Chemical composition | Whether it is within the grade range (the required alloying elements differ by grade) |
| Tensile · yield · elongation · reduction of area | Whether they are at or above the grade minimum and compared against the criteria for the delivered diameter range |
| Hardness | For grades with upper and lower limits, both |
| Impact | For low-temperature grades, the test temperature and absorbed energy value |
| Heat treatment | Quenching and tempering temperatures (for grades with a minimum tempering temperature) |
| Coating | Whether the test is of the pre-coating condition, and whether a plating or coating certificate exists separately |
The layout of fields differs by manufacturer. The group codes of steel certificates (A · B · C · D · Z) are from EN 10168.
Checks for BOMs and buying
- If there is only the bar steelmaker's mill certificate and no product test by the bolt manufacturer, the properties after heat treatment and thread machining are not guaranteed.
- If copies of the same certificate keep being attached to multiple lots, compare the heat number and the marking one by one.
- If plating or PTFE coating was applied later, the mill certificate gives the results before coating. Receive the coating certificate (including baking records for high-strength products) separately.
- CMTR, MTC, and mill certificate differ only in name. Check the EN 10204 type and the issuing party rather than the name.
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: EN 10204 · EN 10168 · ISO 16228 · ISO 898-1 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.