A-286 (UNS S66286)

CommonMaterial

A-286 Iron-Base Precipitation-Hardening Superalloy (UNS S66286)

← Back to topicSend a BOM or RFQ →

Iron-based superalloy hardened by precipitation, with about 25 % Ni and about 15 % Cr plus Ti and others (UNS S66286, commonly A-286). Bolting is sourced as ASTM A453 Grade 660, and bar and forgings as A638 Grade 660.

Key points

  • Corresponding EN 1.4980 (X6NiCrTiMoVB25-15-2) composition: Ni 24.0–27.0, Cr 13.5–16.0, Mo 1.00–1.50, Ti 1.90–2.30, V 0.10–0.50, B 0.0030–0.010, C 0.03–0.08 %, balance Fe.
  • Strength is obtained by solution treatment followed by aging (precipitation hardening) - A453 sets Class A, B, C, and D for Grade 660.
  • Bolting standard: ASTM A453 Grade 660 (Class A, B, C, D). For high-temperature bar and forgings, ASTM A638 Grade 660.
  • Correspondence: JIS SUH660, EN 1.4980 (X6NiCrTiMoVB25-15-2).

Checks for BOMs and buying

  • "A-286" is a common name - order bolts as A453 Grade 660 + Class.
  • Because it is a precipitation-hardening alloy, welding and local heating change its properties.
  • Use a high-temperature lubricant to prevent galling.

Equivalent and superseding standards

  • SUH660 (JIS) · 1.4980 (EN) Corresponding material

ASTM: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: ASTM A453/A453M · ASTM A638/A638M · EN 10269 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.