Mo-containing austenitic stainless steel. UNS S31600, EN 1.4401, and JIS SUS316 correspond to each other, and the low-carbon type 316L is S31603, 1.4404, and SUS316L.
Key points
- Corresponding EN 1.4401 (X5CrNiMo17-12-2): C 0.07 % or less, Cr 16.5–18.5, Ni 10.0–13.0, Mo 2.00–2.50 %.
- 316L (S31603): low-carbon type - the corresponding EN 1.4404 has C 0.030 % or less, and ISO 3506 also allows the "L" designation (for example, A4L-80) for austenitic fasteners with C 0.030 % or less.
- It is not hardened by heat treatment, and strength is raised by cold working - A193 provides the solution-treated or strain-hardened-after-solution-treatment condition, and ISO 3506 treats A4-80 and above as strain-hardened products.
- Correspondence: JIS SUS316 / EN 1.4401 (X5CrNiMo17-12-2); for 316L, SUS316L / 1.4404 (X2CrNiMo17-12-2). 316Ti is 1.4571.
Checks for BOMs and buying
- For a specification that says only "316L bolt", also specify and confirm the strength grade (B8M Class, A4-70, etc.).
- Confirm the distinction between 304 and 316 (presence of Mo) by certificate and PMI, not by a magnet.
ASTM: official search ↗ · ISO: official search ↗
These links go to the issuing bodies; they are not the verification source of individual values.