A phenomenon in which tensile stress and a specific corrosive environment act together on a susceptible material, and branched cracks grow even under low load. For bolts, the clamp load itself is a large tensile stress, so choosing a material suited to the environment is important.
Key points
- It occurs when three things overlap: a susceptible material, tensile stress and a specific environment, and clamp load and residual stress are included in the tensile stress.
- Austenitic stainless steel (304, 316, B8, B8M, A2, A4) is prone to chloride SCC in warm chloride environments. Typical cases are wet piping under insulation and coastal atmosphere.
- Duplex and super duplex steels and alloys with high nickel content resist chloride SCC better than austenitic steels, and are used for bolting on seawater and chloride equipment.
- For high-strength carbon and low-alloy steels, the problems are sulfide stress cracking (SSC) in H2S environments and cracking from hydrogen in service, and these are managed by hardness limits.
- SCC is known for copper alloys such as brass in ammonia, and for carbon steel in concentrated caustic soda.
Checks for BOMs and buying
- For stainless steel bolting wrapped with insulation, watch for chlorides leaching out of the insulation.
- Do not use 304 or 316 bolts in high-temperature seawater and chloride equipment on the judgment that "stainless steel does not rust".
- Over-tightening well beyond the design clamp load increases the SCC risk.
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: NACE MR0175/ISO 15156 · NUREG/CR-7030 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.