2-phase austenitic-ferritic stainless steel. Bolting is specified by ASTM A1082 (high-strength precipitation-hardening and duplex stainless steel bolting).
Key points
- 2205 (UNS S31803, S32205): about 22Cr-5Ni-3Mo-N - corresponds to EN 1.4462 (X2CrNiMoN22-5-3) and JIS SUS329J3L.
- Super duplex 2507 (UNS S32750): about 25Cr-7Ni-4Mo-N - corresponds to EN 1.4410 (X2CrNiMoN25-7-4) and JIS SUS327L.
- Bolting standard: ASTM A1082/A1082M (high-strength precipitation-hardening and duplex stainless steel bolting).
- Correspondence (JSSA table, not a guarantee of equivalence): S31803, S32205 <-> EN 1.4462 · SUS329J3L, S32750 <-> EN 1.4410 · SUS327L.
Checks for BOMs and buying
- In subsea cathodic protection zones, there is a risk of hydrogen-induced stress cracking (HISC) of duplex - check design guidelines such as DNV-RP-F112 and the specification.
- Do not mix carbon steel nuts and washers with duplex bolts (galvanic and reduced corrosion resistance).
- When using in high-temperature equipment, check the temperature upper limit of the applicable code.
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: ASTM A1082/A1082M · EN 10088-1 · DNV-RP-F112 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.