Standard that defines conditions for resistance to sulfide stress cracking (SSC) of metallic materials in oil and gas production equipment containing H2S. For carbon steel and low-alloy steel, hardness of 22 HRC or below is the basic condition.
Status: Current
Key points
- 3-part structure: Part 1 general principles, Part 2 carbon steel and low-alloy steel, Part 3 corrosion-resistant alloys (CRA), etc.
- NACE MR0175 and ISO 15156 are joint standards with the same content. NACE merged with SSPC in 2021 to become AMPP.
- For carbon steel and low-alloy steel, hardness of 22 HRC or below is generally the basic condition.
- Refinery process environments use the separate standard NACE MR0103 / ISO 17945.
Checks for BOMs and buying
- For a line that has B7 and 2H together with "NACE", check against the specification whether it is a grade with limited hardness.
- The hardness range of ISO 898-1 8.8 (22–34 HRC) exceeds the 22 HRC limit, so it does not guarantee the hardness condition for sour-exposed bolting.
- Do not confuse MR0175 (production) with MR0103 (refining).
- Check the specification on whether bolting whose atmospheric exposure is blocked by insulation, burial or flange protection covers is also treated as exposed bolting.
ASTM: official search ↗ · ISO: official search ↗
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: ISO 15156-1 · ISO 15156-2 · ISO 15156-3 · NACE MR0175 · ASTM A193/A193M · ISO 898-1 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.