Type 304 / 304L Austenitic Stainless Steel (UNS S30400 / S30403)

← Back to topicSend a BOM or RFQ →

Austenitic stainless steel with about 18 % Cr and about 8–10 % Ni (18-8). UNS S30400, EN 1.4301, and JIS SUS304 correspond to each other, and the low-carbon type 304L is S30403, 1.4307 (or 1.4306), and SUS304L.

Key points

  • Corresponding EN 1.4301 (X5CrNi18-10): C 0.07 % or less, Cr 17.0–19.5, Ni 8.0–10.5 %.
  • 304L (S30403): low-carbon type - the corresponding EN 1.4307 has C 0.030 % or less, and ISO 3506 also allows the "L" designation for C 0.030 % or less.
  • It is not hardened by heat treatment, and strength is raised by cold working - A193 provides the solution-treated or strain-hardened-after-solution-treatment condition, and ISO 3506 treats A2-80 as a strain-hardened product.
  • Correspondence: JIS SUS304 / EN 1.4301 (X5CrNi18-10); for 304L, SUS304L / 1.4307 (X2CrNi18-9) - 1.4306, with slightly higher Ni, is also used as a 304L family material.

Checks for BOMs and buying

  • For a BOM that says only "SUS bolt", also check whether it is 304 or 316 and the strength grade (B8 Class, A2-70).
  • Cold-worked products can be magnetic - do not judge by a magnet.

ASTM: official search ↗ · ISO: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: EN 10269 · EN 10088-1 · ISO 3506-1 · ASTM A193/A193M · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.