boltnoteSend an RFQ →

Home › Standards glossary › Material and strength grades › A193 B8 (Class 1·2)

A193 B8 (Class 1·2)

ASTMGrade

ASTM A193 Grade B8 (Type 304 Stainless Steel Bolting), Classes 1, 1A, 2 and 2B

← Back to topicSend a BOM or RFQ →

Type 304 austenitic stainless steel bolting grade of ASTM A193. Class 1 is solution-treated with a minimum tensile strength of 75 ksi (converted 517 MPa); Class 2 is strain-hardened and raises this up to 125 ksi at 3/4" or less, but it falls as the diameter gets larger.

Status: Current

Key points

  • When ordering strain-hardened austenitic steel, A193 directs the buyer to understand Appendix X1 thoroughly.
  • Class 1 (solution-treated): minimum tensile/yield 75/30 ksi (converted 517/207 MPa), elongation 30 %.
  • Class 2 (strain-hardened after solution treatment): falls by diameter from 125/100 ksi at 3/4" or less to 100/50 ksi at 1-3/8" to 1-1/2" (table).
  • The diameter of Class 2 is judged by the thread diameter of the finished product, not the bar stock - ASME Interpretation BPV II-A-22-07 (SA-193, applicable to the 2017 edition).
  • ASME VIII-1 Interpretation VIII-77-09 (1977): at high temperature, Class 2 also loses the strength obtained by strain hardening, so the same allowable stress as Class 1 is used.

A193 B8 minimum strength by Class

Class · diameterTensile minYield minElongation min
Class 1 · all diameters75 ksi (converted 517 MPa)30 ksi (converted 207 MPa)30 %
Class 2 · 3/4" or less125 ksi (converted 862 MPa)100 ksi (converted 689 MPa)12 %
Class 2 · 7/8" to 1"115 ksi (converted 793 MPa)80 ksi (converted 552 MPa)15 %
Class 2 · 1-1/8" to 1-1/4"105 ksi (converted 724 MPa)65 ksi (converted 448 MPa)20 %
Class 2 · 1-3/8" to 1-1/2"100 ksi (converted 689 MPa)50 ksi (converted 345 MPa)28 %

Checked against public technical data from 3 or more manufacturers and distributors; not yet checked against the original standard. Reduction of area and hardness are omitted because of differences between sources or too few sources to check against. MPa values are converted.

Checks for BOMs and buying

  • Austenitic studs and nuts gall easily - apply an anti-seize compound and tighten slowly.
  • For a BOM that says only "B8", check the Class - at the same 3/4" or less, the minimum tensile strength differs by 50 ksi between Class 1 and 2.
  • Some specifications require SH and Cl. 2 marking on both ends of Class 2 for field identification (NASA Stennis Space Center piping standard SSTD-8070-0047-PIPE).

ASTM: official search ↗ · ASME: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: ASTM A193/A193M · ASTM A320/A320M · ASTM A194/A194M · ASME interpretation BPV II-A-22-07·VIII-77-09 · NASA SSC SSTD-8070-0047-PIPE · Cross-checked against three or more manufacturer and distributor datasheets (not yet checked against the original standard) · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.