Type 316 (Mo-containing) austenitic stainless steel bolting grade of ASTM A193. Class 1 is solution-treated with a minimum tensile strength of 75 ksi (converted 517 MPa), and strain-hardened Class 2 has separate values by diameter.
Status: Current
Key points
- A193 treats austenitic steel in the solution-treated or strain-hardened-after-solution-treatment condition, and directs the buyer to understand Appendix X1 thoroughly when ordering strain-hardened products.
- Class 1 (solution-treated): minimum tensile/yield 75/30 ksi (converted 517/207 MPa), elongation 30 % - the same as B8 Class 1.
- For Class 2 the strength falls as the diameter gets larger, and the diameter is judged by the thread diameter of the finished product - ASME Interpretation BPV II-A-22-07 (SA-193, applicable to the 2017 edition).
- ASME VIII-1 Interpretation BPV VIII-1-19-10 (2019): SA-193 B8M2 in Table UHA-23 is read as Class 2B - Class 2 and 2B are different classifications.
- Unlike B8, which is 304, B8M contains Mo and is mainly used in chloride environments; the mating nut is A194 8M.
Checks for BOMs and buying
- Class 2 values differ between public sources (a minimum tensile strength of 110 ksi and one of 125 ksi are both given for 3/4" or less) - confirm with the applicable edition's table and the certificate.
- Stainless steel nuts and studs risk galling - use an anti-seize compound.
ASTM: official search ↗ · ASME: official search ↗
These links go to the issuing bodies; they are not the verification source of individual values.
Basis: ASTM A193/A193M · ASTM A194/A194M · ASME interpretation BPV II-A-22-07·BPV VIII-1-19-10 · Cross-checked against three or more manufacturer and distributor datasheets (not yet checked against the original standard) · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.