A453 Grade 660 (A-286)

ASTMGrade

ASTM A453 Grade 660 (UNS S66286) High-Temperature Bolting

← Back to topicSend a BOM or RFQ →

ASTM A453 Grade 660 high-temperature bolting made of A-286 (UNS S66286), a Fe-Ni-Cr precipitation-hardening iron-based superalloy. A453 sets Class A, B, C, and D for Grade 660.

Status: Current

Key points

  • Alloy: an iron-based precipitation-hardening alloy with about 25 % Ni and about 15 % Cr plus Ti, Mo, V, and B - the corresponding EN 1.4980 has Ni 24.0-27.0, Cr 13.5-16.0, and Ti 1.90-2.30 %.
  • Heat treatment: solution treatment followed by aging (precipitation hardening). The solution treatment and aging conditions differ by Class.
  • A453 covers nuts, washers, and screws as well as bolts and studs.
  • Corresponding materials: JIS SUH660, EN 1.4980 (X6NiCrTiMoVB25-15-2).
  • NACE MR0175/ISO 15156-3 Table A.26 places UNS S66286 in the solution-treated and aged (or 2-step aged) condition at 35 HRC or less (NACE interpretation MP 2017-04).

Checks for BOMs and buying

  • "A-286" is a common name - in the order, write A453 Grade 660 together with the Class (A, B, C, D).
  • If the Class is omitted, the strength criterion cannot be known - A453 sets the yield strength by Class, and the overall range is 50-120 ksi (345-825 MPa in the metric edition).
  • Because it is an austenitic alloy, galling occurs easily - use a high-temperature anti-seize compound.

ASTM: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: ASTM A453/A453M · EN 10269 · NACE MR0175/ISO 15156 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.