Bolt fatigue

CommonConcept

Fatigue of bolted joints

← Back to topicSend a BOM or RFQ →

Bolt fatigue arises when cyclic load acts on the stress concentration at the thread root. The fatigue amplitude limit of a thread is tens of MPa, almost independent of strength grade, so the remedy is preload, stiffness and bending control rather than higher strength.

Key points

  • Failure occurs most often at the first thread engaged by the nut, followed by the thread runout (incomplete thread portion) and the radius under the head.
  • With sufficient preload, the share of the external cyclic load carried by the bolt becomes small, Φ·P. If preload is insufficient and the joint interface opens, the whole load acts on the bolt and life drops sharply.
  • Fatigue limit amplitude of bolts rolled before heat treatment (VDI 2230): σASV ≈ 0.85 × (150/d + 45) MPa (d in mm). M16 ≈ 46 MPa, M24 ≈ 44 MPa. It is set by diameter alone and is almost independent of strength grade.
  • Rolled threads retain compressive stress at the root surface and resist fatigue cracks (NASA RP-1228). The formula above is based on bolts rolled before heat treatment.
  • Improvements: high and even preload, lowering bolt stiffness with long, slender (reduced-shank) bolts, rounded root (UNR, UNJ), eliminating bending with a parallel bearing face or spherical washer, preventing fretting on contact surfaces.
  • The axial load fatigue test method is ISO 3800.
  • A fatigue fracture surface shows streaks spreading from the origin (beach marks) and the final fracture zone.

Checks for BOMs and buying

  • Replacing a fatigue-failed bolt with one a grade higher in strength usually does not solve it. Look first at insufficient preload, bending and stiffness causes.
  • Hot-dip galvanizing and some coatings can lower fatigue strength. Check when adding a coating to rotating machinery bolting.
  • For bolts of rotating machinery couplings, connecting rods and bearing caps, check the reuse count and elongation criteria in the equipment manual.
  • Do not substitute a general-purpose bolt for a bolt specified "rolled after heat treatment" on the drawing.

ISO: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: VDI 2230-1 · ISO 3800 · NASA RP-1228 · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.