boltnoteSend an RFQ →

Home › Standards glossary › Inspection, traceability and documents › Tensile test (tensile strength · yield strength · elongation)

Tensile test (tensile strength · yield strength · elongation)

CommonTest

Tensile test (tensile strength, yield strength, elongation, reduction of area)

← Back to topicSend a BOM or RFQ →

A test that pulls a specimen or a whole bolt until it breaks to measure tensile strength, yield strength, elongation, and reduction of area. The TS · YS · EL · RA fields on a certificate are these results.

Key points

  • Tensile strength is the maximum load divided by the cross-sectional area, and yield strength is usually set at the 0.2 % permanent deformation point (0.2 % offset, Rp0.2).
  • Bolts are measured in two ways: product tensile, which pulls the whole product (based on the stress area of the threaded portion), and tensile of a specimen machined from the bolt or bar. Yield strength, elongation, and reduction of area are mainly measured on specimens.
  • Test methods are in ASTM A370 · F606/F606M (fasteners), ISO 898-1 (metric property classes, including test methods), and ISO 6892-1 (metallic materials in general).
  • The overview of the current edition of ASTM A193 covers full-size wedge tensile testing of the product together with specimen tensile requirements. In the wedge test, it must not break at the head-shank junction.

Reading the tensile fields on a certificate

Certificate notationMeaningISO symbol
TS · UTSTensile strengthRm
YS (0.2 % offset)Yield strengthRp0.2 (or ReL)
ELElongation (%)A
RAReduction of area (%)Z

Checks for BOMs and buying

  • When comparing elongation with the standard minimum, check that the gauge length of the specimen is the same as that standard's basis.
  • The tensile values on a bar certificate are based on that bar's diameter. For products of a diameter different from the certificate, check again against the criteria by diameter range.
  • Some grades have only a minimum, but others have an upper limit (e.g., F3125 A490 has tensile 150–173 ksi). A value that is too high may also fail.
  • When converting ksi to MPa, 1 ksi = 6.895 MPa.

ASTM: official search ↗ · ISO: official search ↗

These links go to the issuing bodies; they are not the verification source of individual values.

Basis: ASTM A370 · ASTM F606/F606M · ISO 898-1 · ISO 6892-1 · ASTM A193/A193M · RCSC Specification (2025) · library-wide review 2026-10 (no per-item review date). Project edition, tolerances and service conditions must be confirmed against the standard text and supplier documents. Do not estimate unconfirmed values.